Grades | Stainless Steels | A 965 S20910

SAE A 965 S20910 ( Austenite )

PDF | Word | Print

A 965 S20910 Application:Steel Forgings, Austenitic, for Pressure and High Temperature Parts

Chemical composition(mass fraction)(wt.%) of the A 965 S20910
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Mn 4.00 6.00
Si - 1.00
P - 0.04
S - 0.03
Cr 20.50 23.50
Ni 11.50 13.50
Mo 1.50 3.00
N 0.20 0.40
Nb 0.10 0.30
V 0.10 0.30

Mechanical properties of grade A 965 S20910

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
428 (≥) 422 (≥) 24 21 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade A 965 S20910

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
363 (≥) 964 (≥) 41 23 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
879 311 515 - - -

A 965 S20910 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED