Grades | Stainless Steels | S21500

AISI S21500 ( Austenite )

PDF | Word | Print

S21500 Application:Austenitic Chromium Manganese Nickel Molybdenum Stainless Steel

Chemical composition(mass fraction)(wt.%) of the S21500
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.06 0.15
Si 0.20 1.20
Mn 5.50 7.50
P - 0.04
S - 0.03
Cr 14.0 16.0
Ni 9.00 11.0
Mo 0.80 1.02
Nb 0.75 1.25
V 0.15 0.40
B 0.003 0.009

Mechanical properties of grade S21500

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
713 (≥) 675 (≥) 14 44 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade S21500

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
665 (≥) 253 (≥) 24 23 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
157 297 695 - - -

S21500 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED