Grades | Stainless Steels | S41001

AISI S41001 ( Martensite )

PDF | Word | Print

S41001 Application:Chromium Super Strength Steel

Chemical composition(mass fraction)(wt.%) of the S41001
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn - 1.00
Si - 1.00
P - 0.025
S - 0.025
Cr 11.50 13.50
Ni - 0.75
Mo - 0.50
Al - 0.05
Cu - 0.05
Sn - 0.05

Mechanical properties of grade S41001

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
237 (≥) 271 (≥) 14 12 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade S41001

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
125 (≥) 611 (≥) 11 12 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
745 493 674 - - -

S41001 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED