Grades | Stainless Steels | S32550

AISI S32550 ( Austenitic-Ferritic(Duplex steel) )

PDF | Word | Print

S32550 Application:Duplex (Austenitic-Ferritic) Chromium Nickel Molybdenum Copper Nitrogen Stainless Steel

Chemical composition(mass fraction)(wt.%) of the S32550
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Mn - 1.50
Si - 1.00
P - 0.04
S - 0.03
Cr 24.00 27.00
Ni 4.50 6.50
Mo 2.90 3.90
Cu 1.50 2.50
N 0.10 0.25

Mechanical properties of grade S32550

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
939 (≥) 841 (≥) 11 21 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade S32550

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
367 (≥) 685 (≥) 34 21 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
676 827 942 - - -

S32550 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED