Grades | Stainless Steels | A 988 S32654

SAE A 988 S32654 ( Austenite )

PDF | Word | Print

A 988 S32654 Application:Hot Isostatically-Pressed Stainless Steel Flanges, Fittings, Valves, and Parts for High Temperature Service

Chemical composition(mass fraction)(wt.%) of the A 988 S32654
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn 2.00 4.00
Si - 0.50
P - 0.03
S - 0.005
Cr 24.00 25.00
Ni 7.00 8.00
Cu 0.30 0.60
N 0.45 0.55

Mechanical properties of grade A 988 S32654

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
425 (≥) 795 (≥) 23 23 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 222

Physical properties of grade A 988 S32654

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
367 (≥) 379 (≥) 44 43 21 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
421 244 177 - - -

A 988 S32654 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED