Grades | Stainless Steels | X 30 CrMoN 15-1, X30CrMoN15-1, 1.4108

AWS X 30 CrMoN 15-1, X30CrMoN15-1, 1.4108

PDF | Word | Print

X 30 CrMoN 15-1, X30CrMoN15-1, 1.4108 Application:Stainless steels for rolled and forged products

Chemical composition(mass fraction)(wt.%) of the X 30 CrMoN 15-1, X30CrMoN15-1, 1.4108
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.25 0.35
Si - 1.00
Mn - 1.00
P - 0.030
S - 0.020
Cr 14.00 16.00
Mo 0.85 1.10
Ni - 0.30
N 0.30 0.45

Mechanical properties of grade X 30 CrMoN 15-1, X30CrMoN15-1, 1.4108

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
796 (≥) 929 (≥) 34 43 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 222

Physical properties of grade X 30 CrMoN 15-1, X30CrMoN15-1, 1.4108

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
198 (≥) 624 (≥) 14 31 21 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
315 812 851 - - -

X 30 CrMoN 15-1, X30CrMoN15-1, 1.4108 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED