Grades | Stainless Steels | A 167 Type 310Cb

SAE A 167 Type 310Cb ( Austenite )

PDF | Word | Print

A 167 Type 310Cb Application:Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip

Chemical composition(mass fraction)(wt.%) of the A 167 Type 310Cb
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.50
Mn - 2.00
P - 0.045
S - 0.03
Cr 24.00 26.00
Ni 19.00 22.00
Nb+Ta - 1.10

Mechanical properties of grade A 167 Type 310Cb

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
179 (≥) 919 (≥) 12 41 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade A 167 Type 310Cb

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
329 (≥) 211 (≥) 31 13 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
713 755 129 - - -

A 167 Type 310Cb Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED