Grades | Tool Die Steels | H43

SAE H43

PDF | Word | Print

H43 Application:Hot-Work Tool Steel

Chemical composition(mass fraction)(wt.%) of the H43
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.50 0.65
Si 0.20 0.45
Mn 0.20 0.40
Cr 3.75 4.50
Mo 7.75 8.50
V 1.80 2.20
W - -

Mechanical properties of grade H43

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
967 (≥) 371 (≥) 14 43 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade H43

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
776 (≥) 161 (≥) 13 31 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
988 875 522 - - -

H43 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED