Grades | Tool Die Steels | W112 Extra

SAE W112 Extra

PDF | Word | Print

W112 Extra Application:Tool and die steels

Chemical composition(mass fraction)(wt.%) of the W112 Extra
Elements Min.(≥) Max.(≤) Similar Remarks
C 1.10 1.30
Si 0.10 0.40
Mn 0.10 0.40
Cr - -
V - -

Mechanical properties of grade W112 Extra

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
198 (≥) 898 (≥) 12 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade W112 Extra

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
316 (≥) 357 (≥) 44 31 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
382 796 346 - - -

W112 Extra Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED