T72302 Application:Carbon tool steel products which include hot or cold finished bar, plate, sheet, rod, wire, or forgings, which are normally fabricated into tools, dies, or fixtures.

Chemical composition(mass fraction)(wt.%) of the T72302
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.70 1.50
Si 0.10 0.40
Mn 0.10 0.40
P - -
S - -
Cr - 0.30
V - 0.10
Mo - 0.10
Cu - 0.20
W - 0.15

Mechanical properties of grade T72302

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
847 (≥) 443 (≥) 34 23 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade T72302

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
715 (≥) 678 (≥) 13 32 22 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
593 743 686 - - -

T72302 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED