Grades | Structural Steel | 35 NC 6

DIN 35 NC 6

PDF | Word | Print

35 NC 6 Application:Structural and constructional steels

Chemical composition(mass fraction)(wt.%) of the 35 NC 6
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.33 0.39
Si 0.10 0.40
Mn 0.60 0.90
P - 0.035
S - 0.035
Cr 0.85 1.15
Ni 1.2 1.6

Mechanical properties of grade 35 NC 6

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
788 (≥) 234 (≥) 11 23 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade 35 NC 6

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
637 (≥) 469 (≥) 22 34 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
322 685 383 - - -

35 NC 6 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED