Grades | Special Alloy | BX9Л
ГОСТ BX9Л
BX9Л Application:High temperature alloy castings
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | W(%) | Co(%) | B(%) | Nb(%) | Al(%) | Ti(%) | Other(%) |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 0.02- 0.1 | 0.4 | 0.5 | Max 0.015 | 0.01 | 30.0- 35.0 | Balance | 2.9- 3.5 | 4.7- 5.3 | 0.2- 0.8 | 0.005 | 0.7- 5.3 | 1.0- 1.6 | 0.7- 1.3 | Ca 0.02 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | HBW |
|---|---|---|---|---|---|---|
| 641 (≥) | 134 (≥) | 11 | 34 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 232 |
| Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
|---|---|---|---|---|---|
| 678 (≥) | 748 (≥) | 23 | 33 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc |
| Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
- | - | - |
| 482 | 925 | 211 | - | - | - |
| Product type | Products | Dimension | Processes | Deliver Status |
|---|---|---|---|---|
| Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
| Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |