EN EN X5BCrMnNiN20-8

Location » Home » Grades > Special Alloy > EN X5BCrMnNiN20-8

Grades | Special Alloy | EN X5BCrMnNiN20-8

EN EN X5BCrMnNiN20-8

Print

EN X5BCrMnNiN20-8 Application:Euronorm Stainless Steel

Chemical composition(mass fraction)(wt.%) of the EN X5BCrMnNiN20-8
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%)
0.50-0.60 Max 0.25 7.00-10.0 0.045 0.030 19.5-21.5 1.50-2.75

Mechanical properties of grade EN X5BCrMnNiN20-8

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
166 (≥) 453 (≥) 42 11 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade EN X5BCrMnNiN20-8

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
643 (≥) 257 (≥) 13 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
434 544 157 - - -

EN X5BCrMnNiN20-8 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED