Grades | Special Alloy | EN X46Cr13
EN EN X46Cr13
EN X46Cr13 Application:Euronorm Stainless Steel
Chemical composition(mass fraction)(wt.%) of the EN X46Cr13
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) |
---|---|---|---|---|---|
0.43-0.50 | 1.00 | 1.00 | 0.040 | 0.015 | 12.5-14.5 |
Mechanical properties of grade EN X46Cr13
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | HBW |
---|---|---|---|---|---|---|
427 (≥) | 935 (≥) | 41 | 33 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 432 |
Physical properties of grade EN X46Cr13
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
---|---|---|---|---|---|
258 (≥) | 383 (≥) | 32 | 32 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
- | - | - |
751 | 943 | 574 | - | - | - |
EN X46Cr13 Range of products
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |