17-4PH(UNS S17400) AMS 5604 hot extruded tube pipe

Here's what we're working on and thinking about at Vincie.web

Products | Tube Pipe | 17-4PH(UNS S17400) AMS 5604 hot extruded tube pipe

17-4PH(UNS S17400) AMS 5604 hot extruded tube pipe



17-4 PH is a martensitic, chromium-nickel-copper precipitation-hardening stainless steel 17-4 PH stainless steel is capable of attaining a wide range of strength and toughness properties depending on the precipitation or aging temperature used in hardeni


Delivery Date


Delivery status: Hot-Rolled 、Solutioned 、
Surface:
Standard: ASTM
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other


17-4PH(UNS S17400) AMS 5604 Tube /  Pipe is a martensitic, chromium-nickel-copper precipitation-hardening stainless steel. 17-4 PH stainless steel is capable of attaining a wide range of strength and toughness properties depending on the precipitation or aging temperature used in hardening.  Its valuable combination of  high strength, good corrosion resistance and toughness in both base metals and welds gives designers opportunities to add reliability to their products while simplifying fabrication and often reducing costs. High strength is maintained to approximately 600°F (316°C). This material has good resistance to stress corrosion cracking in the lower strength conditions. 

17-4PH(UNS S17400) AMS 5604 hot extruded tube pipe Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded