50CrVD spring steel strip coil



50CrVD Good mechanical properties and process properties, high hardenability, adding vanadium to refine the grain of steel, reduce overheat sensitivity, improve strength and toughness, high fatigue strength


Delivery Date


Delivery status: Cold-Rolled 、Q+T 、
Surface: Bright 、
Standard: Select
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other


50CrVD alloy spring steel, 50CrVD Good mechanical properties and process properties, high hardenability, adding vanadium to refine the grain of steel, reduce overheat sensitivity, improve strength and toughness, high fatigue strength, yield ratio Higher, but poor weldability and low cold deformation plasticity. It is a higher-grade spring used as a high-load important spring with a large cross section and a valve spring, piston spring, safety valve spring, etc. with an operating temperature <300 °C.

 
US brand: G61500
Japanese brand: SUP10
British brand: 735A51
French brand: 50CrV4

50CrVD spring steel strip coil Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded