1.4923(X22CrMoV12-1) Stainless Steel Sheets/Strip/Plate/Coil



ESR 1 4923 ( X22CrMoV12-1 ) stainless steel sheets, thickness 2 5mm, cold rolled, annealed, bright finish Products used to the manufacturing of high temperature disc springs


Delivery Date


Delivery status: Cold-Rolled 、
Surface: Bright 、
Standard: DIN
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other


ESR L 1.4923( X22CrMoV12-1) Stainless Steel Sheets/Strip/Plate/Coil, Dim. T:0.1-12mm*10-1000mm*L, cold rolled, annealed, bright finish Products used to the manufacturing of high temperature disc springs.

1.4923(X22CrMoV12-1) Stainless Steel Sheets/Strip/Plate/Coil Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded