1.2365(H10, X32CrMoV3-3, SKD7) Hot-Work Mould Steel

Here's what we're working on and thinking about at Vincie.web

Products | Tool Die Steels | 1.2365(H10, X32CrMoV3-3, SKD7) Hot-Work Mould Steel

1.2365(H10, X32CrMoV3-3, SKD7) Hot-Work Mould Steel



1 2365(H10, X32CrMoV3-3, SKD7) Hot-Work Mould Steel


Delivery Date


Delivery status: Forged 、Q+T 、
Surface: Milling 、
Standard: DIN
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other



1.2365(H10, X32CrMoV3-3, SKD7) Hot-Work Mould Steel is a hot working tool steel in the ASTM A681 standard for alloy tool steels. ASTM / AISI classifies chrome hot tool steels as Group H steels ranging from H10, H11, h12 to H19. AISI H10 tool steel is one of the chrome hot work tool steels with excellent softening resistance at high temperatures.

 
H10 tool steel can be heat treated to make it harder than tungsten hot work steel and has higher toughness. H10 tool steel has good thermal fatigue characteristics. Unlike tungsten hot work steel, 1.2365(H10, X32CrMoV3-3, SKD7) Hot-Work Mould Steel can be safely water cooled in use.
 
1.2365(H10, X32CrMoV3-3, SKD7) Hot-Work Mould Steel is recommended for hot working tools such as hot punches, die casting dies, forging dies, hot scissor blades, hot clamping dies and extrusion dies.
 

USA German Japan British
ASTM A681 DIN EN ISO 4957 JIS G4404 BS 4659
H10/T20810 1.2365/32CrMoV12-28 SKD7 BH10

1.2365(H10, X32CrMoV3-3, SKD7) Hot-Work Mould Steel Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded