422(UNS S42200, 616, 1 4935) Stainless Steel BarAlloy 422 stainless bar is a hardenable, martensitic stainless steel designed for service temperatures as high as 1200 F This grade develops high mechanical properties via heat treatment and offers good sca


Delivery Date


Delivery status: Forged 、Q+T 、Ageing 、
Surface: Bright 、Milling 、
Standard: AMS
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other


422(UNS S42200, 616, 1.4935) Stainless Steel Bar  is a hardenable, martensitic stainless steel designed for service temperatures as high as 1200 F.
This grade develops high mechanical properties via heat treatment and offers good scaling and oxidation resistance. 
Typical applications have included buckets and blades in steam turbines, high temperature bolting and valve and valve trim.

UNS S42200
AMS 5655
ASTM A 176
ASTM A 565
AMSE SA 176
B50A951 A1
B50A951 A2
AISI 636
SAE AMS 5655

422 stainless
Alloy 422
422
Inventory Size Range
Bar : 0.500" - 13.000"
Standard Inventory Lengths: 10-12 feet rl's.
The technical data provided is for information only and not for design purposes. It is not warranted or guaranteed.
Common Applications of Alloy 422 Stainless Steel
Power Generation
Compressors
Steam turbines
Aircraft parts
High-temperature bolting

Mechanical Properties of 422(UNS S42200, 616, 1.4935) 
422(UNS S42200, 616, 1.4935)  bar is readily machinable in the annealed condition with machining characteristics similar to those of 422(UNS S42200, 616, 1.4935)  stainless steel.

422(UNS S42200, 616, 1.4935) Stainless Steel Bar Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded

Enquiry