410CB Stainless Steel Forging Flat bar

Here's what we're working on and thinking about at Vincie.web

Products | Stainless Steels - Special Steels | 410CB Stainless Steel Forging Flat bar

410CB Stainless Steel Forging Flat bar



410Cb is an AOD + ESR melted martensitic stainless steel alloy This alloy has elevated strength and toughness as


Delivery Date


Delivery status: Forged 、Q+T 、
Surface: Bright 、Milling 、
Standard: ASTM
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other


410Cb is an AOD + ESR melted martensitic stainless steel alloy. 
This alloy has elevated strength and toughness as compared to standard 410.  The addition of columbium allows for improved grain size control and greater ease in heat treating. This grade is

410CB Stainless Steel Forging Flat bar Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded

Enquiry