By 50 t, 3 LF electric arc furnace smelting furnace t electrode, electroslag remelting, insulation, annealing, 800 650 * 4 mill production process leaves Phi 180 steel refining, casting (%: 0 06 ~ 0 15C, 0 25 ~ 0 80M 11 25 ~ 13 n, 00C R, M o = 0 30, 60N


Delivery Date


Delivery status: Forged 、Q+T 、
Surface: Milling 、
Standard: Select
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other


By 50 t, 3 LF electric arc furnace smelting furnace t electrode, electroslag remelting, insulation, annealing, 800 /650 * 4 mill production process leaves Phi 180 steel refining, casting (%: 0.06 ~ 0 15C, 0.25 ~ 0.80M 11.25 ~ 13 n, 00C R, M o = 0.30, 60N = 0 I less than or equal to 0, 025P, 0.010S). The electric furnace smelting ingredients into the dephosphorizing agent, Bachu all LF dross. After refining argon blowing, A line and C a - S I line were finally deoxidized. After analysis, the technical indexes meet the standard requirements

Steel of Turbine blade B50A947 A4 Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded