Grades | Superalloys | INCONEL® alloy MA 758
AMS INCONEL® alloy MA 758
PDF | Word | Print
INCONEL® alloy MA 758 Application:It is used in a range of thermal processing applications, from furnace components, such as hearth rollers, to jigs, tools, and other fabrications for supporting workpieces through heat-treatment processes. It has been specified for a fuel atomizer applica
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | - | 0.05 | |
Cr | - | - | 30.00 | |
Al | - | - | 0.30 | |
Ti | - | - | 0.50 | |
Yttrium oxide (Y2O3) | - | - | 0.60 | |
Fe | - | - | 1.00 | |
Ni | - | - | Bal |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | HBW |
---|---|---|---|---|---|---|
225 (≥) | 234 (≥) | 31 | 41 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 433 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
---|---|---|---|---|---|
963 (≥) | 594 (≥) | 33 | 41 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
- | - | - |
535 | 645 | 528 | - | - | - |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |