Grades | Special Alloy | ЖC3-BИ
ГОСТ ЖC3-BИ
ЖC3-BИ Application:Standard vacuum smelting casting high temperature alloy
Si(%) | Mn(%) | P(%) | S(%) | V(%) | B(%) |
---|---|---|---|---|---|
Max 0.6 | Max 0.6 | Max 0.015 | Max 0.009 | Max 0.3 | 0.005-0.010 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | HBW |
---|---|---|---|---|---|---|
797 (≥) | 682 (≥) | 41 | 21 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 411 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
---|---|---|---|---|---|
149 (≥) | 156 (≥) | 33 | 41 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
- | - | - |
212 | 257 | 346 | - | - | - |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |