BЖЛ8 Application:Russia TY standard grades and chemical compositions of the high temperature alloy castings

Chemical composition(mass fraction)(wt.%) of the BЖЛ8
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.20
Cr 14.80 17.00
Al 2.50 3.50
Mo 4.50 6.00
Ti 1.80 2.50
Co - -
W - -
Ni - remaining
Nb - -
Fe 8.00 12.00
B - 0.06
Ce - 0.010
V - -
Zr - -
Mn - 0.60
Si - 0.70
S - 0.015
P - 0.020

Mechanical properties of grade BЖЛ8

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
134 (≥) 351 (≥) 11 41 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade BЖЛ8

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
142 (≥) 915 (≥) 33 23 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
789 491 168 - - -

BЖЛ8 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED