Grades | Stainless Steels | ЖC3-BИ

GOST ЖC3-BИ

PDF | Word | Print

ЖC3-BИ Application:Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(mass fraction)(wt.%) of the ЖC3-BИ
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.11 0.16
Cr 14.00 18.00
Ni - remaining
Co - -
Mo 3.00 4.50
W 4.50 6.50
Al 1.60 2.20
Ti 1.60 2.30
Nb - -
Fe - 8.00

Mechanical properties of grade ЖC3-BИ

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
596 (≥) 151 (≥) 31 44 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade ЖC3-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
816 (≥) 586 (≥) 32 33 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
332 776 867 - - -

ЖC3-BИ Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED