Grades | Stainless Steels | 12X8BΦ

GOST 12X8BΦ ( Martensite )

PDF | Word | Print

12X8BΦ Application:Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(mass fraction)(wt.%) of the 12X8BΦ
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.15
Si - 0.60
Mn - 0.50
P - 0.030
S - 0.025
Cr 7.00 8.50
Ni - 0.60
Mo - 0.20
W 0.60 1.00
Ti - 0.03
V 0.30 0.50

Mechanical properties of grade 12X8BΦ

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
819 (≥) 635 (≥) 23 44 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade 12X8BΦ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
533 (≥) 465 (≥) 13 23 21 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
661 272 521 - - -

12X8BΦ Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED