- AFNOR 55NiCrMoV7
- AFNOR 55NiCrMoV7
- AFNOR 55CrNiMoV 4
- AFNOR 55CrNiMoV 4
- AFNOR 45CrMoV6
- AFNOR 45CrMoV6
- AFNOR 0NiCrMoV16
- AFNOR 0NiCrMoV16
- AFNOR 40NiCrMo16
- AFNOR 40NiCrMo16
- AFNOR 40CrMoV13
- AFNOR 40CrMoV13
- AFNOR 35NiCrMoV8
- AFNOR 35NiCrMoV8
- AFNOR 35CrMo8
- AFNOR 35CrMo8
- AFNOR X2NiCoMoTi18-8-5
- AFNOR X2NiCoMoTi18-8-5
- AFNOR X1CrNiMoAl12-9
- AFNOR X1CrNiMoAl12-9
- AFNOR X100CrMo17
- AFNOR X54Cr14
- AFNOR X54Cr14
- AFNOR X44Cr14
- AFNOR X40Cr14
- AFNOR X40Cr14
- AFNOR X38CrMo16-1
- AFNOR X38CrMo16-1
- AFNOR X33Cr13
- AFNOR X33Cr13
- AFNOR X20Cr13
- AFNOR X20Cr13
- JIS 60Si8
- JIS 60Si8
- AFNOR 51Si7