- GBT 17Cr18Ni9
- GBT S30103
- GBT 022Cr17Ni7
- GBT S35550
- GBT 20Cr15Mn15Ni2N
- GBT S35020
- GBT 20Cr13Mn9Ni4
- GBT S35950
- GBT 10Cr17Mn9Ni4N
- GBT S38340
- GBT 16Cr25Ni20Si2
- GBT S38240
- GBT 16Cr20Ni14Si2
- GBT S33010
- GBT 12Cr16Ni35
- GBT S32590
- GBT 45Cr14Ni14W2Mo
- GBT S31020
- GBT 20Cr25Ni20
- GBT S30920
- GBT 16Cr23Ni13
- GBT 22Cr21Ni12N
- GBT S35850
- GBT 22Cr20Mn10Ni2Si2N
- GBT S35750
- GBT 26Cr18Mn12Si2N
- GBT S35650
- GBT 53Cr21Mn9Ni4N
- GBT S38148
- GBT 06Cr18Ni13Si4
- GBT S34778
- GBT 06Cr18Ni11Nb
- GBT S32168
- GBT 06Cr18Ni11Ti
- GBT S31793