- AMS SA-813 S34709
- AMS SA-240 S34709
- AMS SA-965 S34700
- AMS SA-814 S34700
- AMS SA-813 S34700
- AMS SA-358 S34700
- AMS SA-240 S34700
- AMS SA-479 S34565
- AMS SA-409 S34565
- AMS SA-376 S34565
- AMS SA-358 S34565
- AMS SA-312 S34565
- AMS SA-249 S34565
- AMS SA-240 S34565
- AMS SA-213 S34565
- AMS SA-240 S33400
- AMS SA-479 S33228
- AMS SA-312 S33228
- AMS SA-240 S33228
- AMS SA-213 S33228
- AMS SB-710 N08330
- AMS SB-536 N08330
- AMS SB-535 N08330
- AMS SB-511 N08330
- AMS SA-688 S32654
- AMS SA-479 S32654
- AMS SA-358 S32654
- AMS SA-312 S32654
- AMS SA-249 S32654
- AMS SA-240 S32654
- AMS SA-965 S32109
- AMS SA-814 S32109
- AMS SA-813 S32109
- AMS SA-403 S32109
- AMS SA-240 S32109